Chlorinated rubber paint has good weather resistance and can effectively resist the influence of harsh environmental factors such as wind, rain, and ultraviolet rays, maintaining a long service life.
The coating has the characteristics of water resistance and moisture resistance, and is suitable for metal surfaces used in humid environments.
Good acid, alkali, and salt spray resistance, suitable for painting in acidic, alkaline, and salt corrosive environments, and suitable for metal surfaces used in chemical environments.
The product has good coating adhesion, single component packaging, easy construction, and can be applied by various methods such as brush coating, roller coating, spray coating, etc.
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() | ![]() |
Chlorinated rubber paint is widely used for anti-corrosion coating on various metal surfaces.
Including: steel structures, doors and windows, railings, stairs, building steel structures, etc
Ship: hull, deck, cabin, etc
Petrochemical industry: storage tanks, pipelines, valves, etc
Agricultural machinery: agricultural implements, tractors, etc
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
To be applied as a topcoat on steel surfaces and concrete surfaces in coastal areas and corrosive environments. For example, wharf piers, steel structure facilities, factory steel structures, chemical storage tanks, oil tanks, open-air oil and water pipelines, lighthouses, cement chimneys, etc.
| Color | Near color sample |
|---|---|
| Mixed density | 1.3 kg/L (white and light colors) |
| Film thickness | Dry film 40 microns, wet film 100 microns |
| Theoretical usage | 0.14 kg/m ² (based on a dry film of 40 microns)Q |
| Flash point | 31°C |
| Drying time | Surface dry h ≤ 0.5 hours, actual dry h ≤ 5 hours |
| Covering power (g/m ² ≤) | White 110, Red 150, Black 40, Medium Grey 80, Milk Yellow 140, Fruit Green 100, Emerald 90, Deep Yellow 140 |
Water resistance, soaking for 24 hours | No bubbles, no peeling. |
The topcoat uses chlorosulfonated polyethylene, chlorinated rubber, high chlorinated polyethylene, epoxy, acrylic polyurethane, and fluorocarbon external magnetic paint.

The surface of the coated steel must be thoroughly cleaned of oil stains, oxide scales, rust, old coatings, etc. Shot blasting or sandblasting methods can be used, with a rust removal standard of Sa2.5 and a roughness of 40-75 μ m; Manual polishing and rust removal methods can also be used, with a rust removal standard of St2.0 level and a dull metallic luster exposed on the surface.
1.Smoking and open flames (including lighters and matches), welding, cutting, and other operations that generate sparks or high temperatures are strictly prohibited at the construction site and surrounding areas.
2.Adequate ventilation: Maintaining air circulation in the workplace is the most effective way to dilute flammable and toxic gases.
3.Eye protection: Wear chemical protective goggles or face shields.
4.If paint accidentally touches the skin, immediately rinse thoroughly with soap and plenty of water.
Store in a dry and cool environment, away from heat and fire sources. The storage area must be well ventilated and equipped with fire extinguishers.
This manual is our testing and practical experience, which can be used as a reference for construction. With the continuous improvement and updates of the iron red epoxy rust primer product and materials, please request the latest data for accuracy.

Address: No. 7, Cowboy City 2nd Road, Xintang Town, Zengcheng District, Guangzhou (Room 1011, Building A3, Zhongmao International Building)
Service Hotline:1333-2829-075
Tel:020-32913637
E-mail:kaigetl@163.com