Glass flakes are tightly arranged in the paint film, forming a dense and continuous shielding layer, effectively blocking the contact between corrosive media and substrates, and resisting corrosion from chemical media such as acid, alkali, salt, seawater, atmosphere, and various oils.
Glass flakes have high hardness and strength, which can enhance the mechanical properties of the paint film, making it wear-resistant, impact resistant, and prolonging its service life.
Epoxy resin has good adhesion and can firmly adhere to various substrates.
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() | ![]() |
Petrochemical:Tanks, pipelines, valves, instruments, etc.Electricity:Power plant transmission lines, substations, cables, etc.
Metallurgy:Steel plants, electroplating plants, pickling tanks, etc.Ship:Ship's inner shell, ballast tank, oil tank, etc.
Bridge:Bridge steel box girders, bridge piers, anti-collision railings, etc.Other:Sewage treatment facilities, seawater aquaculture facilities, etc.
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Suitable for long-term heavy-duty anti-corrosion intermediate coating on steel structural components, equipment and facilities, and concrete components in highly corrosive environments. For example, sewage treatment tanks, storage tanks, offshore platforms, port facilities, offshore pile pipes, etc. need to be coated with a heavy-duty anti-corrosion supporting system.
| Color | Adjustable color |
|---|---|
| Mixed density | 1.45~1.50 kg/L |
| Film thickness | Dry film 100 microns, wet film 170 microns |
| Theoretical usage | 0.26 kg/m ² (based on a dry film of 100 microns) |
| Flash point | 27°C |
| Drying time | Surface dry h ≤ 4 hours, actual dry h ≤ 24 hours |
| Mixing ratio | Component A: Component B=5:1 (weight ratio) |
Maturity period | 10 minutes |
| Usage period after mixing | 3 hours |
| Soak in 3% saltwater for 68 hours | No bubbles, no peeling, no rust stains |
The topcoat uses chlorosulfonated polyethylene, chlorinated rubber, high chlorinated polyethylene, epoxy, acrylic polyurethane, and fluorocarbon external magnetic paint.

The surface of the coated steel must be thoroughly cleaned of oil stains, oxide scales, rust, old coatings, etc. Shot blasting or sandblasting methods can be used, with a rust removal standard of Sa2.5 and a roughness of 40-75 μ m; Manual polishing and rust removal methods can also be used, with a rust removal standard of St2.0 level and a dull metallic luster exposed on the surface.
1.Smoking and open flames (including lighters and matches), welding, cutting, and other operations that generate sparks or high temperatures are strictly prohibited at the construction site and surrounding areas.
2.Adequate ventilation: Maintaining air circulation in the workplace is the most effective way to dilute flammable and toxic gases.
3.Eye protection: Wear chemical protective goggles or face shields.
4.If paint accidentally touches the skin, immediately rinse thoroughly with soap and plenty of water.
Store in a dry and cool environment, away from heat and fire sources. The storage area must be well ventilated and equipped with fire extinguishers.
This manual is our testing and practical experience, which can be used as a reference for construction. With the continuous improvement and updates of the iron red epoxy rust primer product and materials, please request the latest data for accuracy.

Address: No. 7, Cowboy City 2nd Road, Xintang Town, Zengcheng District, Guangzhou (Room 1011, Building A3, Zhongmao International Building)
Service Hotline:1333-2829-075
Tel:020-32913637
E-mail:kaigetl@163.com
Web:https://www.kaigepaint.com